3D Compound Inspector

← Back

Blast Furnace (Iron Extraction)

Category: Chemistry

Level: SS3

Syllabus topic: SS3 Extraction of Metals

Formula: Fe₂O₃ + 3CO → 2Fe + 3CO₂

Description: A detailed cutaway model of an industrial blast furnace used for smelting iron from haematite ore (Fe₂O₃). Showcases the double bell charging hopper at the throat, descending charge burden (iron ore, coke, and limestone flux), refractory firebrick lining within the steel mantle, golden bustle pipe distributing hot air blast through tuyères into the hearth combustion zone (~1800 °C), and the tapping levels separating denser molten pig iron from floating calcium silicate slag.

📝 Exam Key Points
  1. Raw materials (Charge burden): Haematite ore (Fe₂O₃), Coke (C, fuel & reducing agent source), Limestone (CaCO₃, flux), and preheated blast air.
  2. Combustion zone (Hearth/Bosh, ~1800 °C): C + O₂ → CO₂ (highly exothermic heat source), followed by reduction: CO₂ + C → 2CO.
  3. Reduction of Haematite (Stack, 400–700 °C): Fe₂O₃(s) + 3CO(g) → 2Fe(l) + 3CO₂(g).
Saved on this device.

Blast Furnace (Iron Extraction)

Fe₂O₃ + 3CO → 2Fe + 3CO₂

Chemistry · SS3

Syllabus topic: SS3 Extraction of Metals

Key Exam Points

  1. Raw materials (Charge burden): Haematite ore (Fe₂O₃), Coke (C, fuel & reducing agent source), Limestone (CaCO₃, flux), and preheated blast air.
  2. Combustion zone (Hearth/Bosh, ~1800 °C): C + O₂ → CO₂ (highly exothermic heat source), followed by reduction: CO₂ + C → 2CO.
  3. Reduction of Haematite (Stack, 400–700 °C): Fe₂O₃(s) + 3CO(g) → 2Fe(l) + 3CO₂(g).

Student Notes

Scan to view the 3D model